- Outer Dimensions: 19.05mm – 114.3mm
- Wall Thickness: 2.0mm – 14 mm
- Length: max 16000mm
Application: Seamless and Welded Steel Pipe for Low-Temperature Service.
Steel grade: ASTM A333 Grade 1
Packing: Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.
Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test.
Surface treatment: Oil-dip, Varnish, Passivation, Phosphating, Shot Blasting.
Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.
Packing: Bare packing/bundle packing/crate packing/wooden protection at the both sides of tubes and suitably protected for sea-worthly delivery or as requested.
Inspection and Test: Chemical Composition Inspection, Mechanical Properties Test(Tensile Strength,Yield Strength, Elongation, Flaring, Flattening, Bending, Hardness, Impact Test), Surface and Dimension Test,No-destructive Test, Hydrostatic Test.
Surface treatment: Oil-dip, Varnish, Passivation, Phosphating, Shot Blasting.
Both ends of each crate will indicate the order no., heat no., dimensions, weight and bundles or as requested.
ASTM A333 Grade 1 Chemical Compositions(%)
Compositions | Data |
Carbon(max.) | 0.30 |
Manganese | 0.40–1.06 |
Phosphorus(max.) | 0.025 |
Sulfur(max.) | 0.025 |
Silicon | … |
Nickel | … |
Chromium | … |
Other Elements | … |
Mechanical properties for ASTM A333 Grade 1 Alloy Steel
Properties | Data |
Yield strength(min) | 205Mpa |
Tensile strength(min) | 380Mpa |
Elongation(%) | 35 |
Strike Temperature Condition for ASTM A333 Grade 1
The lowest temperature for strike test | |
℉ | ℃ |
-50 | -45 |
Other ASTM Standards
- A262 Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
- A941 Terminology Relating to Steel, Stainless Steel, Related Alloys, and Ferroalloys
- A1016/A1016M Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes
- E112 Test Methods for Determining Average Grain Size